品名 |
類別 |
AWS型號 |
純?nèi)鄯蠼饘倩瘜W(xué)成分% |
特性及用途 | ||||||||
C |
Si |
Mn |
Cr |
Ni |
N |
Mo |
P |
S | ||||
不銹鋼焊絲 |
308L |
ER308L |
<=0.02 |
0.4 |
1.75 |
20 |
10 |
0.4 |
|
<=0.05 |
<=0.015 |
焊接18Cr-8Ni不銹鋼,電弧穩(wěn)定,由于增加了Si的含量,焊接操作性及烙金流動性更佳 |
308LSi |
ER308LSi |
<=0.02 |
0.8 |
1.75 |
20 |
10 |
|
|
<=0.025 |
<=0.005 |
焊接18Cr-8Ni不銹鋼電弧穩(wěn)定,焊道美觀,抗裂性強(qiáng),由于增加了Si的含量,焊接操作性及熔金流動性更佳 | |
308H |
ER308H |
0.06 |
1 |
1.75 |
20 |
10 |
|
<=0.5 |
<=0.03 |
<=0.02 |
焊接18Cr-8Ni 不銹鋼,電弧穩(wěn)定,焊道美觀,抗裂性強(qiáng) | |
307Si |
ER307Si |
<=0.1 |
0.8 |
7 |
19.5 |
9 |
|
|
|
|
錳含量高故裂紋敏感度低,適用于非磁性鋼,高錳鋼,硬化性耐磨鋼等難以焊接的鋼材 | |
307 |
ER307 |
<=0.05 |
0.5 |
6 |
18 |
8 |
|
|
<=0.025 |
<=0.0015 |
適用于硬化鋼、磁性鋼及其他難以焊接的鋼材 | |
309L |
ER309L |
0.02 |
0.4 |
1.7 |
23.5 |
13.5 |
|
|
<=0.025 |
<=0.015 |
異種金屬焊接用,耐熱腐蝕性佳,電弧穩(wěn)定,作業(yè)性良 | |
309LSi |
ER309LSi |
<=0.03 |
0.8 |
1.8 |
23.5 |
13.5 |
|
|
<=0.022 |
<=0.015 |
異種金屬焊接用,耐熱耐蝕性佳,電弧穩(wěn)定,作業(yè)性良,由于增加了Si的含量,焊接操作性及熔金流動性更佳 | |
309Si |
ER309Si |
<=0.03 |
0.8 |
1.7 |
23.5 |
13.5 |
|
|
<=0.022 |
<=0.015 |
異種金屬焊接用,耐熱耐蝕性佳,電弧穩(wěn)定,作業(yè)性良 | |
309LMo |
ER309LMo |
0.02 |
0.4 |
1.5 |
21.5 |
12.5 |
|
2.7 |
|
|
高溫耐熱裂和腐蝕性好,焊接金屬為超低碳奧氏體組織,適用于低碳鋼與不銹鋼的異種金屬焊接 | |
310 |
ER310 |
<=0.12 |
0.35 |
1.8 |
26 |
21 |
|
<=0.30 |
<=0.015 |
<=0.015 |
熔金含25Cr-20Ni,多用于310S不銹鋼的焊接比KMS,309更適合異種金屬焊接及自硬性高的合金鋼和高碳鋼之焊接 | |
312 |
ER312 |
<=0.12 |
0.4 |
1.8 |
30 |
9 |
|
0.3 |
<=0.025 |
<=0.015 |
用異種鋼之焊接,其裂紋敏感度低,故焊接覆面鋼等鋼材,不銹鋼里襯,焊接困難或易發(fā)生氣孔 | |
316L |
ER316L |
<=0.02 |
0.5 |
1.8 |
18.5 |
11.5 |
0.4 |
2.6 |
<=0.025 |
<=0.015 |
焊接18Cr-12Ni-Mo2超低碳不銹鋼,焊接工藝性好,抗晶間腐蝕性能優(yōu)良 | |
316LSi |
ER316LSi |
<=0.02 |
0.8 |
1.8 |
18.5 |
12 |
0.045 |
2.7 |
<=0.025 |
<=0.015 |
焊接18Cr-12Ni-Mo2超低碳不銹鋼,焊接工藝性好,抗晶間腐蝕性能優(yōu)良,由于增加了Si的含量,焊接操作性及熔金流動性更佳 | |
317L |
ER317L |
0.02 |
0.4 |
1.8 |
19 |
13.5 |
|
3.6 |
|
|
超低碳含量及含Mo高,抗晶間腐蝕,高溫強(qiáng)度大 | |
318 |
ER318 |
<=0.05 |
0.4 |
1.4 |
19 |
11.5 |
|
2.7 |
<=0.020 |
<=0.015 |
適用于18Cr-12Ni-2.5Mo-Ti鋼,工作溫度可達(dá)400℃抗晶間腐蝕性能優(yōu)良 | |
318Si |
ER318Si |
<=0.05 |
0.8 |
1.4 |
19 |
11.5 |
|
2.7 |
<=0.020 |
<=0.015 |
適用于18Cr-12Ni-2.5Mo-Ti鋼,抗晶間腐蝕性能優(yōu)良,由于增加了Si的含量,焊接操作性及熔金流動性更佳 | |
347 |
ER347 |
<=0.055 |
0.45 |
1.4 |
19.5 |
9.5 |
0.045 |
|
<=0.025 |
<=0.015 |
因添加了Nb等合金元素,故焊道晶間腐蝕抵抗性能增強(qiáng),且具有極佳之高溫強(qiáng)度,特別適用于耐熱鋼之焊接 | |
347Si |
ER347Si |
<=0.055 |
0.8 |
1.4 |
19.5 |
9.5 |
0.045 |
|
<=0.025 |
<=0.015 |
因添加了Nb等合金元素,焊道晶間腐蝕抵抗性能增強(qiáng),且具有極佳之高溫強(qiáng)度,特別適用于耐熱鋼之焊接,由于增加了Si的含量,焊接操作性及熔金流動性更佳 | |
2209 |
ER2209 |
<=0.03 |
1 |
2.5 |
22.5 |
8.5 |
0.15 |
3 |
<=0.03 |
<=0.02 |
適用于22Cr-9Ni-Mo3的雙相不銹鋼,如UNS31803 | |
904L |
ER385 |
<=0.03 |
1 |
<=0.01 |
20.5 |
34 |
|
2.5 |
<=0.03 |
<=0.02 |
適用于20Cr-25Ni-4.5Mo-1.5Cu不銹鋼,特別耐腐蝕 | |
409 |
ER409Cb |
<=0.05 |
0.6 |
0.7 |
11.5 |
<=0.60 |
|
<=0.50 |
<=0.030 |
<=0.030 |
適用于409,410不銹鋼的焊接 | |
410 |
ER410 |
<=0.12 |
0.6 |
<=1.00 |
12.5 |
<=0.60 |
|
|
<=0.035 |
<=0.030 |
用于焊接410或420系列不銹鋼,硬化性大,具有高溫抗氧化、抗腐蝕性,應(yīng)用于石油精練及化學(xué)工業(yè)及堆焊修補(bǔ) | |
410NiMo |
ER410NiMo |
<=0.03 |
0.4 |
0.4 |
11.7 |
4.5 |
0.4 |
0.5 |
<=0.025 |
<=0.015 |
用于焊接410或420系列不銹鋼,硬化性大,具有高溫抗氧化、抗腐蝕生,應(yīng)用于石油精練及化學(xué)工業(yè)及堆焊修補(bǔ) | |
420 |
ER420 |
<=0.34 |
0.5 |
<=1.00 |
12.5 |
<=0.60 |
|
<=0.75 |
<=0.040 |
<=0.030 |
適用于13Cr或17Cr馬氏體不銹鋼之焊接 | |
430 |
ER430 |
>=0.04 |
<=0.5 |
0.45 |
16.5 |
<=0.60 |
|
|
<=0.030 |
<=0.015 |
適用于13Cr或17Cr馬氏體不銹鋼之焊接,應(yīng)用于汽車工業(yè) |